Advanced Material Unsaturated Polyester Resin

Fire Retardant Resins

GRADE NO. TYPE VISCOSITY (Pa.s) GEL TIME (25℃,min) PROPERTIES AND APPLICATIONS
CSJ-1905 Additive Type 0.20-0.35 10.1-30.5 Additive and fire-retardant resin, possess halogen-free, low-smoke and high fire-retardant performance, FRP oxygen index: 30.
CSJ-1906 Additive Type 0.55-1.1 18.0-38.0 Additive and fire-retardant resin, low-smoke and good fire-retardant performance, FRP oxygen index: 30.
CSJ-1908 Reactive Type 0.3-0.6 7.1-15.5 Reactive and fire-retardant resin, excellent mechanical property and fire-retardant performance, FRP oxygen index: 30.
CSJ-1909 Reactive Type 0.3-0.6 10.0-20.0 Reactive and fire-retardant resin, excellent mechanical property and fire-retardant performance, FRP oxygen index: 30.